The best treatment is the one matched to the wear mechanism. HVOF tungsten carbide (100–400 μm) suits low-impact sliding abrasion with tight tolerances. PTA hardfacing (1.5–5 mm, NiCrBSi + 40–65% WC) suits abrasive duty with impact because the thick metallurgical bond resists spalling. Hardox or AR plate as the base flight provides full-section wear reserve when a coating alone is insufficient.
Identify whether the flight experiences impact from tramp metal, coarse lumps or high feed rates. A thin, very hard coating on a soft substrate can collapse under load or crack under impact. A thick weld overlay on a low-impact application may add cost without proportional life gain. The process choice follows the mechanism, not a universal “hardest material" rule.
HVOF deposits WC-CoCr at 100–400 μm with low heat input. Suitable for tight-tolerance surfaces and low-impact wear.
PTA hardfacing deposits NiCrBSi + WC at 1.5–5 mm with a metallurgical bond. Suitable for screw flights, mixers and crushers.
Weld hardfacing with chromium or complex carbides reaches 3–10 mm and is economical for large areas but generates more heat and distortion.
Flight wear concentrates on the outer edge on the pushing side. Hardfacing only that band, rather than the full face, concentrates the wear material where it is needed while retaining core toughness. A Winding Spiral Blade Forming Machine can produce the base geometry; the hardfacing follows as a separate operation.
Hardfacing typically extends wear life 2–5* over bare steel when correctly applied. A combined solution—CDP spiral flight, tungsten carbide hardfacing on shaft and edges, and polymer encapsulation—extended life from 7–10 months to 24–28 months in a pulp application. These gains depend on matching the process to the actual wear condition.